How Is Vickers Hardness Measured: Diagonals and Test Loads

How Is Vickers Hardness Measured: Diagonals and Test Loads

How Is Vickers Hardness Measured: The Indentation and the Two Diagonals

The question of how is Vickers hardness measured comes down to one geometric idea: a diamond pyramid is pressed into the surface, and the size of the mark it leaves is converted into a hardness number. The indenter is a square-based pyramid with a defined apex angle, so the footprint on the specimen is a square rotated by 45 degrees. After the load is removed, the operator measures the two diagonals of that footprint with a measuring microscope or an image analysis system.

The hardness value is calculated from the applied test force divided by the contact area of the indentation, which is derived from the mean of the two diagonals. Because the diagonals are measured in both directions, a slightly asymmetric indentation caused by surface tilt or local anisotropy is averaged out rather than ignored. This is why careful specimen preparation matters so much: a blurred or rounded indent edge shifts the diagonal reading and therefore the result.

Test loads are chosen in steps rather than freely. Low-force and micro ranges are used for thin sections, coatings and individual phases, while heavier loads are used for bulk metal where a larger, more representative footprint is wanted. The load and the diagonal measurement are inseparable — the same material tested at two different loads is not directly comparable unless the standard’s requirements for load selection are respected. Equipment for this work sits within the broader family of metallographic hardness testing systems, which pair the hardness machine with the mounting and polishing line needed to prepare the surface.

Standards and Specimen Preparation Behind the Measurement

ISO 6507-1 covers Vickers hardness testing and is the reference document for the indenter geometry, the force ranges and the measurement procedure. It is a different document from ISO 6508-1, which covers Rockwell hardness testing, and from ASTM E18, which covers Rockwell hardness testing of metallic materials. Confusing the three is a common source of mismatched results between laboratories, because each defines its own indenter, force sequence and reporting requirements.

Surface Finish, Mounting and Edge Quality

The indentation diagonals can only be measured as accurately as the surface allows. Metallographic polishing sequences commonly use diamond suspensions from 9 um down to 0.25 um, finished with 0.05 um colloidal silica. Where a small specimen needs to be held securely, hot mounting embeds it in thermosetting resin at about 150-180 C under pressure, which protects the edge and keeps the indentation square to the viewing axis.

Specimen thickness relative to indentation depth, the distance from the indent centre to the specimen edge, and the spacing between adjacent indents are all controlled by the standard rather than left to the operator. A reading taken too close to an edge or on a specimen that is too thin is not a valid Vickers result, even if the arithmetic is correct. For laboratories that also run tensile and impact work, the same preparation discipline carries across the metal testing machines used for those methods.

Results should always be quoted with the standard, the test force, the specimen preparation route and the measuring device used. Without that context, two numbers that look identical may not be comparable at all.

Equipment Selection and the Measurement Workflow

A Vickers hardness machine combines a rigid frame, a calibrated force application system, an objective lens and a measuring eyepiece or camera. Force calibration is verified in the same spirit as uniaxial machine verification under ISO 7500-1 and ASTM E4, where the indicated force must stay within a defined tolerance of the true force. Load cells in that context are commonly supplied as class 0.5 or class 1 per ISO 7500-1, meaning the indicated force stays within +/-0.5 % or +/-1 % of the true force.

Capacity selection follows the specimen and the standard, exactly as it does for tensile frames: a 1000 kN machine is not suitable for a sample that needs 1 N of force. The same logic applies to hardness, where the chosen test force must suit the section thickness and the feature being measured. When a laboratory is sizing a universal frame alongside its hardness bench, the UTM capacity selector helps match frame capacity to the specimen rather than to habit.

StepWhat Is ControlledWhy It Matters
Specimen preparationPolishing to 0.05 um colloidal silica finishClean diagonal edges for measurement
Force applicationTest load per ISO 6507-1Valid indentation size for the section
Diagonal measurementBoth diagonals, averagedReduces error from tilt and anisotropy
ReportingStandard, load, preparation routeComparability between laboratories

CHENJI supplies hardness and preparation equipment through chenjitester.com alongside tensile, impact and fatigue frames, so a laboratory can keep one calibration and reporting discipline across methods. Where fasteners are the product, hardness results are often read together with torque and clamp force data from fastener testing applications, since both describe how the part will behave in service.

FAQ

Does changing the Vickers test load change the measured hardness value?

It can, especially at low forces where the indentation is small and surface effects dominate. The load must be selected per ISO 6507-1 for the section thickness, and the load used should always be reported with the result.

How close to the specimen edge can a Vickers indentation be placed?

The standard sets a minimum distance from the indent centre to the edge and between neighbouring indents, scaled to the indentation size. Placing an indent too close to an edge produces a collapsed footprint and an invalid diagonal reading.

Why must the surface be polished before measuring the diagonals?

The diagonals are read optically, so scratches and rounded edges blur the corners of the footprint. A sequence finishing with 0.05 um colloidal silica gives the sharp indent corners needed for a repeatable measurement.

Closing Notes on Repeatable Vickers Results

A Vickers number is only as good as the diagonal measurement and the force that produced it, so preparation, load selection and reporting discipline carry equal weight. Laboratories that standardise all three can compare results across operators and across sites without re-testing. To discuss a hardness bench, a preparation line or a combined metal testing setup, contact annie@chenjitester.com or +86 158 5311 1612, or Request a Quote. Related equipment includes spring testing systems and automotive test benches for components that also require hardness verification.